11 hours ago, plato said:

Another thumbs for acothane DW. Not cheap but did an excellent job. Took nearly 4 litres to do a 1350 litre bow tank. I added the activator to the pot, mixed it thoroughly then decanted it into a fresh paint kettle and mixed it again. No problem with unmixed paint.

BUT you can’t hang around as the mixed product cures pretty fast. 

The fact I bought a new paint kettle for the job and forgot about using it as was so focused in using it in time! So it’s either spots that weren’t mixed well or I used the lid at the end just to use it up without thinkinga. Used 4l on a 1000l tank and also did 2 litres at a time. Wish I had the empty tin from the activator as I reckon I need literally a couple of drops to cure the two tiny tacky areas😒

Link to comment
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
  • Recently Browsing   0 members

    • No registered users viewing this page.
×
×
  • Create New...

Important Information

We have placed cookies on your device to help make this website better. You can adjust your cookie settings, otherwise we'll assume you're okay to continue.